MoSi2 Heating Elements, MoSi2 Heater
Chemical Properties
Add to Basket Inquire now

Chemical_Properties


Oxygen-resistance under high temperature: in oxidizing atmosphere, on the surface of MoSi2 element owing to the high-temperature combustion a layer of compact quartz (SiO2) protective film is formed to prevent MoSi2 from continuously oxidizing. When the element temperature is higher than 1700?, the SiO2 protective film, Whose fusing point is 1710?, is fused, and the SiO2 is fused into molten drops owing to the action of its surface extension, so that loses its protective ability. In the oxidizing atmosphere, when the element is continuously used, again the protective film forms.
It should be pointed out that MoSi2 heat-generating element cannot be used for rather long time in 400-700?, or it will be powdered owing to the strong oxidizing action in low temperature.


[ Contact Info ]
icon Company Songshan Enterprise Group
icon Address Sanlizhuang High & New Tech. Zone, Dengfeng Zhengzhou Henan 452483 China
icon Phone 86 - 371 - 62768046
icon Fax 86 - 371 - 62768249
icon Homepage www.songshangroup.com
icon Contact Yang Xuehao / Imp & Exp Manager  Inquire now
Leave me a message

Add to Favorites Print Recommend to My Friends       
   
 
 
Physical Properties china gold supplier
Copyright(C)2002~2005, Songshan Enterprise Group All right reserved.
Tel: +86-371-62768046 Fax: +86-371-62768249